<font size=3>At 09:42 AM 3/25/2005, you wrote:<br>
</font><blockquote type=cite class=cite cite="">
<font face="Verdana" size=3>Hi Roger, <br>
So you are actually using the PVC-E as a gap-filler to
a large extent, judging from the pic and your description. I guess that
makes sense, as it has enough flexibility/spring when dry to keep from
being noisy,</font></blockquote><br><br>
Hi Fred<br><br>
<blockquote type=cite class=cite cite=""><font face="Verdana" size=3>
like, say tite-bond (how would I know that?) Oh my! did
you you do that silly thing. I would never do that.........
again.(G)</font></blockquote><br><br>
<br>
<blockquote type=cite class=cite cite=""><font face="Verdana" size=3>
Love those felt knuckles. Yep! sells a set
of hammer shanks every time, plus an action weight off. Want to buy
some used lead. It's quality Steinway
lead.</font></blockquote><br>
Regards Roger<br>