A breakthrough on glue

erwinspiano at aol.com erwinspiano at aol.com
Mon Sep 15 09:03:47 MDT 2008



? Mike
? Thanks .? This is really good news?of a time saving product. & one that creates a quality repair.?Thanks for the efforts to include us in your learning curve & offering it for sale.
? Kindest regards
? Dale Erwin



List,

??? At the risk of sounding like a salesman (which I am not), I feel?I must promote a product that we have been using quietly?with great success for many years now, and until?recently unable?to obtain in enough quantity to pass on. ?We all know that there are dozens of ways to glue down new and old ivory and plastic, and there are just as many schools of thought on how to do?so. This list can attest to that and debate it for a decade.

????Blackstone Valley Piano,?as a business dedicated to proper keytop replacement, has the luxury of gluing down?keytops in a workshop?under controlled conditions. We are?not in a clients home with the clock ticking, this changes?the approach.

?

????Our glue (we call it Mineral plastic glue) is a Modified PVA and in most aspects similar to PVC-E. 

Similarities are:

it is water based, non-solvent

designed to bond porous (wood, ivory, bone, cloth, leather) and non-porous (plastics) materials to other porous materials

easy to use, when wet cleans with water

glue line remains flexible

?

??? Where the similarities end, our Modified PVA glue:

dries perfectly white, not clear

produces grain tearing bonds

is thicker and gap filling

?

In our early years we found that when?replacing keytops?on old keyboards, PVC-E glue?was simply to thin. Even after a "primer coat" or?"glue sizing",? we were often stuck with a glue starved joint. After an exhausting search we found the Modified PVA.??When?applying acrylic and mineral plastics, it's thickness allows?enough of the glue to remain?on the surface instead of being immediately?absorbed in, promoting as I stated earlier a "grain tearing bond".

?

If working with new or old ivory,?our? Modified PVA glue dries pure white, so it improves the appearance. This also works out well for people who don't like to use linen wafers or don't like to mix whitener in their glue. PVC-E, hide glue and super glue?do not dry white and allow imperfections to show through the ivory.?This glue's ?thickness and gap filling qualities aid in filling in the little areas on keytops that get ripped out when removing worn heads or tails.?When removing the old ivory and replacing it with plastic,?this glue?can?compensate for?a bit of unevenness on the keytop surface.

?

As I stated earlier, as a business, we?have the advantage of working in a shop under controlled conditions. This glue sets up quickly but requires clamping overnight to fully cure, it is not a fast drying glue to use?on the road or in a clients home. We sell it as "mineral plastic glue" on our website.?

?

?

I'll bring some to the Southeast Regional Conference in October, meanwhile, if this interests anyone or if you need some more information, feel free to contact me on or off the list.? Mike

?

Blackstone Valley piano
Michael A. Morvan
76 Sutton Street
Uxbridge, Ma 01569
(508) 278-9762
www.pianoandorgankeys.com
www.thepianorebuilders.com

?

?

??? 

-------------- next part --------------
An HTML attachment was scrubbed...
URL: https://www.moypiano.com/ptg/pianotech.php/attachments/20080915/25a0709d/attachment-0001.html 


More information about the Pianotech mailing list

This PTG archive page provided courtesy of Moy Piano Service, LLC