<DIV>For sure not all epoxy is equal! I have used the syrenge type epoxies that they sell in hardware stores and find that it does NOT cure as hard as WestSystem. The WestSystem product cures REALLY hard/ridged. Some other kinds are more flexible. </DIV>
<DIV>&nbsp;</DIV>
<DIV>Also epoxy has a shelf life: Don't take chances with old stuff. If its more than a year old toss it! I also try to replace my cyanoacrylate glue every 6 months. <BR><BR><B><I>Stéphane Collin &lt;collin.s@skynet.be&gt;</I></B> wrote:</DIV>
<BLOCKQUOTE class=replbq style="PADDING-LEFT: 5px; MARGIN-LEFT: 5px; BORDER-LEFT: #1010ff 2px solid"><BR><BR>The Araldite I used was in the form of two syringues coupled with one common<BR>push button. Even without intelligence, that would have produced the right<BR>mix, or do I miss something (again) ? And they claimed for optimal adhesion<BR>after 12 hours, foreseen ambiant temperature was above 0°C, which was about<BR>half the time I waited and 20° below actual temperature in the place where<BR>it happened.<BR><BR></BLOCKQUOTE><BR><BR>Ryan Sowers, RPT  Puget Sound Chapter<br>Pianova Piano Service<br>Olympia, WA<p>__________________________________________________<br>Do You Yahoo!?<br>Tired of spam?  Yahoo! Mail has the best spam protection around <br>http://mail.yahoo.com