<p>It is no more dangerous than household bleach, ammonia, CA glue, isopropyl (rubbing) alcohol, airplane glue, contact cement and a lot of other stuff we use in the all-American household. <br /><br />A. Use in well ventilated area<br />B. Avoid getting on skin, wash off if you do<br />C. Don't drink it<br /><br />Alan Barnard<br />Salem, MO<br /><br /></p>
<div style="padding-right: 5px; padding-left: 5px; padding-bottom: 5px; border-left: #000000 3px solid; padding-top: 5px">
<hr />Original message<br />From: "Avery Todd"
<ptuner1@gmail.com></ptuner1@gmail.com><br />To: "Pianotech List"
<pianotech@ptg.org></pianotech@ptg.org><br />Received: 10/2/2007 4:38:48 PM<br />Subject: Re: Hammer softening<br /><br />
<div align="left">Sorry, it's not worth the risk to me! See: <a href="http://en.wikipedia.org/wiki/Methanol">http://en.wikipedia.org/wiki/Methanol</a></div>
<div></div>
<div>Especially scroll on down to the bottom to "Health and Safety". </div>
<div><br />Avery Todd<br /> </div>
<div><span class="gmail_quote">On 10/2/07, <b class="gmail_sendername">Michael Kurta</b> <<a href="mailto:mkurta@roadrunner.com">mkurta@roadrunner.com</a>> wrote:</span>
<blockquote class="gmail_quote" style="padding-left: 1ex; margin: 0px 0px 0px 0.8ex; border-left: #ccc 1px solid">
<div bgcolor="#ffffff">
<div><font face="Tahoma" size="2"> Hi Gary:</font></div>
<div><font face="Tahoma" size="2"> This is a direct quote from the Baldwin service manual:</font></div>
<div><font face="Tahoma" size="2"> "For a Softer Tone: A mixture of 25% water and 75% methanol can be applied to the hammers to produce a mellower tone in Baldwin hammers. Care should be taken not to apply to stapled areas. The solution can be applied to the shoulders for moderate changes or to the strike point for more severe changes. It is recommended in most cases not to apply the solution to the top octave and lowest octave since these areas usually require more tone accentuation to be musically pleasing. It takes about 20-30 minutes for the solution to work. Fine voicing can then be performed with shallow needling to the hammers as needed to provide a consistent note to note tone." </font></div>
<div><font face="Tahoma" size="2"> I've used this solution for years and found it to work well.</font></div>
<div><font face="Tahoma" size="2">Methanol BTW, is non-permanent anti-freeze and can sometimes be found at farm supply stores. Its also found in windshield washer fluid, but I'm not sure what else is in there and the proportion of water to methanol. </font></div>
<div><font face="Tahoma" size="2"></font></div>
<div><font face="Tahoma" size="2"> Mike Kurta, Syracuse chapter </font></div>