<DIV><BR><FONT face=Arial size=2>&gt; Oh, and a practical question about your 
being in the CC <BR>&gt; capital of the universe. When the RH% gets into the low 
teens, <BR>&gt; say 15%, the MC of the soundboards will be 3.5%, at or before 
<BR>&gt; which point a CC board will be flat or have reverse crowned. <BR>&gt; 
Do you have a recognized annual killer octave season or <BR>&gt; festival 
there?<BR>&gt; Ron N<BR>&gt; </FONT></DIV>
<DIV><FONT face=Arial size=2></FONT>&nbsp;</DIV>
<DIV><FONT face=Arial size=2><STRONG><EM>Hmmm, well I like festivals, Maestro, 
but will there be floats...</EM></STRONG></FONT></DIV>
<DIV><FONT face=Arial size=2></FONT>&nbsp;</DIV>
<DIV><FONT face=Arial size=2><STRONG><EM>&nbsp;3.5 to 4% is the emc of choice 
for my CC friends. I've measured a few of these boards so far and surprisingly 
they have plenty of crown, probably coming from a combination of the forced 
crowning from the gobar deck and from the inner rim.</EM></STRONG></FONT></DIV>
<DIV><FONT face=Arial size=2><STRONG><EM></EM></STRONG></FONT>&nbsp;</DIV>
<DIV><FONT face=Arial size=2><STRONG><EM>Whereas I'm at 5%, rib supported. I 
have a wood conditioning room that senses RH and opens a relay that I can 
designate for humidification or dehumidification depending on the season, but in 
all honesty I let her ride down to 4% this time of year rather than put my board 
in a "wet box."</EM></STRONG></FONT></DIV>
<DIV><FONT face=Arial size=2><STRONG><EM></EM></STRONG></FONT>&nbsp;</DIV>
<DIV><FONT face=Arial size=2><STRONG><EM>I also machine a tongue and groove 
joint in my planks. Del Fandrich referred me to the government's Wood Handbook, 
which I read in parts. The text states that while this joint is stronger in 
theory because of the additional glue surface, the effect is often negated by 
poor machining. I make sure I'm getting a great joint on all five sides and 
these panels feel stiffer than side grain edge glued panels. Also the tongue and 
groove allows me to align the planks in such a way that you end up with a 
thicker panel overall, which I don't think can be 
refuted.</EM></STRONG></FONT></DIV>
<DIV><FONT face=Arial size=2><STRONG><EM></EM></STRONG></FONT>&nbsp;</DIV>
<DIV><FONT face=Arial size=2><STRONG><EM>Jude Reveley, RPT<BR>Absolute Piano 
Restoration, LLC<BR>Lowell, Massachusetts<BR>(978) 
323-4545</EM></STRONG></FONT></DIV></BODY></HTML>