formula for Hammer softening solution?

Don drose@dlcwest.com
Mon, 29 Jan 2001 10:35:01 -0600


Hi Carol

The alcohol is a wetting agent--I would try alcohol and water first.
Woolite is just another wetting agent--but one that leaves a residue behind
it. (read oil)

At 11:19 AM 1/29/01 -0500, you wrote:
>I know it's in the archives "somewhere" but what is the formula for hammer 
>softening solution.  I recall it uses Woolite (or some fabric softener) and 
>water?  isopropyl alcohol?  methyl alcohol?
>
>Thanks.
>
>Carol Beigel
>
>_________________________________________________________________
>Get your FREE download of MSN Explorer at http://explorer.msn.com
>
>
>

Regards,
Don Rose, B.Mus., A.M.U.S., A.MUS., R.M.T., R.P.T.

Tuner for the Saskatchewan Centre of the Arts

mailto:drose@dlcwest.com
http://donrose.xoasis.com/

3004 Grant Rd.
REGINA, SK
S4S 5G7
306-352-3620 or 1-888-29t-uner